Erratum to “Successive Orthorhombic Distortions in Kagome Metals by Molecular Orbital Formation”

Advanced Materials
DOI: 10.1002/adma.73192 (Physics and Astronomy)
Licence : non indiquée (tous droits réservés)

Résumé : There was an error in calculating the integrated intensities in Figure 3. To obtain the integrated intensities for the square points (red, blue) above 720 K, a default integration mask with the same size and position was used, with only a difference in the total scaling factor for the red and blue points. Consequently, the critical exponent for the diffuse scattering is revised from γ = 1.1 ( 2 ) $\gamma =1.1(2)$ to γ = 0.9 ( 3 ) $\gamma =0.9(3)$ ; however, the two values agree within error. Also, the diffraction map in the L = 1 $L=1$ plane, instead of L = 3 $L=3$ , was presented for GdRu 3 B 2 ${\rm GdRu}_3{\rm B}_2$ in Figure S2b. The corrected Figures are displayed herein. These corrections do not affect the results or the conclusions of the paper.

Publié le 04 Mai. 2026